Intermediate‐Temperature Environmental Effects on Boron Nitride‐Coated Silicon Carbide‐Fiber‐Reinforced Glass‐Ceramic Composites
Authors:
- 1 March 1997
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 80 (3) , 609-614
Abstract
The environmental effects on the mechanical properties of fiber‐reinforced composites at intermediate temperatures were investigated by conducting flexural static‐fatigue experiments in air at 600° and 950°C. The material that was studied was a silicon carbide/boron nitride (SiC/BN) dual‐coated Nicalon‐fiber‐reinforced barium magnesium aluminosilicate glass‐ceramic. Comparable time‐dependent failure responses were found at 600° and 950°C when the maximum tensile stress applied in the bend bar was 60% of the room‐temperature ultimate flexural strength of as‐received materials. At both temperatures, the materials survived 500 h fatigue tests at lower stress levels. Among the samples that survived the 500 h fatigue tests, a 20% degradation in the room‐temperature flexural strength was measured in samples tested at 600°C, whereas no degradation was observed for the samples tested at 950°C. Microstructure and chemistry studies revealed interfacial oxidation in the samples that were fatigued at 600°C. The growth rate of the Si‐C‐O fiber oxidation product at 600°C was not sufficient to seal the stress‐induced cracks, so that the interior of the material was oxidized and resulted in a strength degradation and less fibrous fracture. In contrast, the interior of the material remained intact at 950°C because of crack sealing by rapid silicate formation, and strength/toughness of the composite was maintained. Also, at 600°C, BN oxidized via volatilization, because no borosilicate was formed.Keywords
This publication has 14 references indexed in Scilit:
- High‐Temperature Tensile Behavior of a Boron Nitride‐Coated Silicon Carbide‐Fiber Glass‐Ceramic CompositeJournal of the American Ceramic Society, 1996
- Flexural Creep of Coated SiC‐Fiber‐Reinforced Glass‐Ceramic CompositesJournal of the American Ceramic Society, 1995
- Environmental ageing effects in a silicon carbide fibre‐reinforced glass‐ceramic matrix compositeJournal of Microscopy, 1995
- Interfacial Microstructure and Chemistry of SiC/BN Dual‐Coated Nicalon‐Fiber‐Reinforced Glass‐Ceramic Matrix CompositesJournal of the American Ceramic Society, 1994
- Oxidation Effects on the Mechanical Properties of a SiC‐Fiber‐Reinforced Reaction‐Bonded Si 3 N 4 Matrix CompositeJournal of the American Ceramic Society, 1992
- Solid Reaction in the MgO Excess Region of the System MgO-TiO2-Al2O3Journal of the Ceramic Society of Japan, 1992
- Oxidation kinetics of SiC deposited from CH3SiCl3/H2 under CVI conditionsJournal of Materials Science, 1992
- Effect of Interfaces on the Properties of Fiber‐Reinforced CeramicsJournal of the American Ceramic Society, 1990
- Fiber–Matrix Interfacial Characteristics in a Fiber‐Reinforced Ceramic‐Matrix CompositeJournal of the American Ceramic Society, 1989
- Structure and chemistry of fibre-matrix interfaces in silicon carbide fibre-reinforced glass-ceramic composites: an electron microscopy studyJournal of Materials Science, 1987