Abstract
The crystallization of calcium chloro‐ and chloro‐fluoroapatites from calcium halide fluxes was studied as a function of composition and heating schedules. Activation of was investigated by varying phosphor stoichiometry and firing methods. The results indicate that flux‐grown apatites are slightly deficient in and that for a particle size of predominantly 50–100μ, 72‐hr firing at 1150°C causes only limited incorporation of Sb3+ , Cd2+, and additional . The incorporation of Mn2+ is more extensive and may be nearly uniform. The rate of migration of Mn and Sb toward the interior of the crystals increases with increasing [as ] added prior to activation; however, maximum emission occurs at a calculated over‐all metal/phosphorus ratio of exactly 5/3. High output of heterogeneously emitting crystals suggests that quantum efficiency is independent of activator concentration.