Effect of Grinding and Multi-Stimuli Aging on the Fatigue Strength of a Y-TZP Ceramic
Open Access
- 1 February 2018
- journal article
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 29 (1) , 60-67
Abstract
This study aimed to investigate the effect of grinding and multi-stimuli aging on the fatigue strength, surface topography and the phase transformation of Y-TZP ceramic. Discs were manufactured according to ISO-6872:2008 for biaxial flexure testing (diameter: 15 mm; thickness: 1.2 mm) and randomly assigned considering two factors “grinding” and “aging”: C- control (as-sintered); CA- control + aging; G- ground; GA- ground + aging. Grinding was carried out with coarse diamond burs under water-cooling. Aging protocols consisted of: autoclave (134°C, 2 bars pressure, 20 hours), followed by storage for 365 days (samples were kept untouched at room temperature), and by mechanical cycling (106 cycles by 20 Hz under a load of 50% from the biaxial flexure monotonic tests). Flexural fatigue strengths (20,000 cycles; 6 Hz) were determined under sinusoidal cyclic loading using staircase approach. Additionally, surface topography analysis by FE-SEM and phase transformation analysis by X-ray Diffractometry were performed. Dixon and Mood methodology was used to analyze the fatigue strength data. Grinding promotes alterations of topographical pattern, while aging apparently did not alter it. Grinding triggered t-m phase transformation without impacting the fatigue strength of the Y-TZP ceramic; and aging promoted an intense t-m transformation that resulted in a toughening mechanism leading to higher fatigue strength for as-sintered condition, and a tendency of increase for ground condition (C < CA; G = GA). It concludes that grinding and aging procedures did not affect deleteriously the fatigue strength of the evaluated Y-TZP ceramic, although, it promotes surface topography alterations, except to aging, and t-m phase transformation.Keywords
This publication has 21 references indexed in Scilit:
- Short‐Term Prospective Clinical Evaluation of Monolithic and Partially Veneered Zirconia Single CrownsJournal of Esthetic and Restorative Dentistry, 2016
- Low-temperature degradation of Y-TZP ceramics: A systematic review and meta-analysisJournal of the Mechanical Behavior of Biomedical Materials, 2016
- Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear simulationJournal of Dentistry, 2015
- Effects of aging procedures on the topographic surface, structural stability, and mechanical strength of a ZrO2-based dental ceramicDental Materials, 2014
- Emerging Ceramic-based Materials for DentistryJournal of Dental Research, 2014
- The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramicsJournal of the European Ceramic Society, 2008
- Low-Temperature Degradation of Zirconia and Implications for Biomedical ImplantsAnnual Review of Materials Research, 2007
- The Strength and Hydrothermal Stability of Y‐TZP Ceramics for Dental ApplicationsInternational Journal of Applied Ceramic Technology, 2007
- Transformation Toughening in Zirconia‐Containing CeramicsJournal of the American Ceramic Society, 2000
- Phase change and mechanical properties of ZrO2-Y2O3 solid electrolyte after ageingSolid State Ionics, 1981