Abstract
This paper describes a way to improve the microstructure and mechanical properties of welding seams by in situ and conventional post‐weld heat treatments for laser beam welding of the Ti–45Al–5Nb–0.2C–0.2B alloy. The seams are crack‐free with reduced longitudinal residual stress and higher elongation to fraction after post‐weld heat treatment. The welding zone consists of α2 after welding, transforms to a massive γ during in situ post‐weld heat treatment, and finally forms a convoluted microstructure after conventional heating. The phase composition across the welding zone is discussed.

This publication has 19 references indexed in Scilit: