Ultrahigh cycle fatigue fracture mechanism of high-quality bearing steel obtained through different deoxidation methods
Authors:
- 6 May 2021
- journal article
- research article
- Published by Springer Nature in International Journal of Minerals, Metallurgy and Materials
- Vol. 28 (5) , 804-815
Abstract
No abstract availableKeywords
This publication has 31 references indexed in Scilit:
- Evolution Mechanism of Non-metallic Inclusions in Al-Killed Alloyed Steel during Secondary Refining ProcessISIJ International, 2013
- Influence of the Inclusion Shape on the Rolling Contact Fatigue Life of Carburized SteelsMetallurgical and Materials Transactions A, 2012
- Top slag refining for inclusion composition transform control in tire cord steelInternational Journal of Minerals, Metallurgy and Materials, 2012
- Effect of inclusion/matrix interface cavities on internal-fracture-type rolling contact fatigue lifeMaterials & Design (1980-2015), 2011
- Behavior of alumina-magnesia complex inclusions and magnesia inclusions on the surface of molten low-carbon steelsMetallurgical and Materials Transactions B, 2001
- Characteristics of Agglomeration of Various Inclusion Particles on Molten Steel Surface.ISIJ International, 1997
- "In-situ" Observation of Collision, Agglomeration and Cluster Formation of Alumina Inclusion Particles on Steel Melts.ISIJ International, 1997
- Experimental Studies on Al2O3 Inclusion Removal from Steel Melts Using Ceramic Filters.ISIJ International, 1995
- An Automatic Ultrasonic Fatigue Testing System for Studying Low Crack Growth at Room and High Temperatures1994
- Quantitative evaluation of effects of non-metallic inclusions on fatigue strength of high strength steels. II: Fatigue limit evaluation based on statistics for extreme values of inclusion sizeInternational Journal of Fatigue, 1989