Repair bond strength of composite: Effect of surface treatment and type of composite
Authors:
- Ss HashemikamangarSHSs Hashemikamangar
- Mj KharazifardMKMj Kharazifard
Open Access
- 1 January 2018
- journal article
- Published by Medicina Oral, S.L. in Journal of Clinical and Experimental Dentistry
- Vol. 10 (6) , e520-e527
Abstract
By an increase in use of composite restorations, some defects are also seen in these restorations, which need to be repaired. Since complete replacement of an old restoration may compromise the tooth structure, repair of defect is a more practical approach if there is no caries recurrence. Risk of pulp injury also decreases as such. One major challenge in restoration repair is to obtain a durable bond between the new and old composite. Laser irradiation has been suggested for surface preparation of old composite. This study aimed to assess the effect of composite surface preparation with Er,Cr:YSGG laser on microtensile bond strength to new composite. A total of 18 blocks were fabricated in three groups of nanohybrid, microhybrid and Beautiful II giomer measuring 4x7x7 mm and subjected to 10,000 thermal cycles between 5-55°C with 30 seconds of dwell time. The samples were randomly assigned to no surface treatment (etching and bonding) or laser plus etching and bonding groups. Composite cylinders measuring 4x7x7 mm were fabricated of Beautiful, nanohybrid and microhybrid composites on old composite surfaces and subjected to 500 thermal cycles for 50 seconds between 5-55°C with 30 seconds of dwell time. Each block was sectioned into 10 samples and they were subjected to microtensile bond strength test. Data were analyzed using ANOVA and Tukey's test. In all composites, the mean bond strength in laser subgroups was higher than that in control subgroups except for giomer, which showed lower bond strength in laser subgroup. The lowest mean bond strength was noted in repair of Z350XT with Z350XT when the surface of old composite was etched (10.92 MPa). The highest mean bond strength was noted in repair of Z250 with giomer when the old composite surface was irradiated with laser (30.55 MPa). Er,Cr:YSGG laser plus etching increased the bond strength in all groups except for giomer group, which showed a reduction in bond strength. Key words:Composite resins, surface treatment, tensile bond strength, laser, er,cr:ysgg, giomer.Keywords
This publication has 27 references indexed in Scilit:
- Effects of three surface conditioning techniques on repair bond strength of nanohybrid and nanofilled compositesDental Research Journal, 2015
- Effect of Surface Treatments on Microtensile Bond Strength of Repaired Aged Silorane Resin CompositeOperative Dentistry, 2013
- An In Vitro Assessment of the Effects of Three Surface Treatments on Repair Bond Strength of Aged CompositesOperative Dentistry, 2011
- Effect of thermocycling on the bond strength of composite resin to bur and laser treated composite resinLasers in Medical Science, 2011
- Effects of surface conditioning on repair bond strengths of non-aged and aged microhybrid, nanohybrid, and nanofilled composite resinsClinical Oral Investigations, 2010
- Effect of surface treatments on the tensile bond strength of repaired water-aged anterior restorative micro-fine hybrid resin compositeJournal of Dentistry, 2008
- Effect of surface conditioning methods on the microtensile bond strength of resin composite to composite after aging conditionsDental Materials, 2007
- Influence of Er:YAG laser on tensile bond strength of a self-etching system and a flowable resin in different dentin depthsJournal of Dentistry, 2004
- Composite–composite repair bond strength: effect of different adhesion primersJournal of Dentistry, 2003
- Bond strength of repaired anterior composite resins: an it>/it> studyJournal of Dentistry, 1998