Influence of glass fiber amount, natural ageing, UV ageing and aged/reprocessed ratios on mechanical, rheological and morphological properties of polycarbonate
Authors:
- 9 June 2026
- journal article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science
- Vol. 240 (19) , 7554-7568
Abstract
In the current research, the influence of reprocessing for aged glass fiber reinforced polycarbonate (PC) composites having different glass fiber amount was investigated on the mechanical properties (tensile, impact, flexural), melt flow index and morphology. Samples were subjected to two environments, namely artificial accelerated aging in a QUV chamber (simulating outdoor weathering with alternating cycles of ultraviolet (UV) light and moisture at controlled elevated temperature) for up to 336 h and natural aging in Gebze (Türkiye) for up to 1 year between August 2017 and August 2018. After these aging stages, naturally and UV aged samples were ground and the ground samples were blended with virgin glass fiber reinforced PC at different ratios (25%, 50% and 75% by weight). Natural aging caused moderate reductions in tensile strength, reaching 2.61%, 7.29%, and 7.82% decreases for 10%, 20%, and 30% glass fiber reinforced composites after 12 months, respectively. Under UV aging, tensile strength remained relatively stable, whereas elongation at break decreased up to 27% depending on fiber content and exposure duration. Flexural strength decreased by up to 13.60% after natural aging, while impact strength reductions reached approximately 20% after prolonged UV exposure. Melt flow index (MFI) values increased significantly after aging and reprocessing, indicating dominant chain scission mechanisms. In particular, 20% glass fiber reinforced exhibited a 122.82% increase in MFI after 9 months of natural aging. Reprocessed aged composites showed further MFI increases and partial recovery in some mechanical properties with virgin material addition; however, the original mechanical performance could not be fully restored. SEM observations revealed increased fiber–matrix debonding, surface cracks, and interfacial gaps after aging and reprocessing. Overall, higher glass fiber contents improved the dimensional and mechanical stability of PC composites against environmental aging, while reprocessing introduced additional degradation associated with fiber shortening and matrix deterioration.Keywords
Funding Information
- Türkiye Bilimsel ve Teknolojik Araştırma Kurumu (116M257)
This publication has 34 references indexed in Scilit:
- Influence of thermo‐oxidative aging on the mechanical properties of the bead foams made of polycarbonate and polypropyleneJournal of Polymer Science, 2023
- Accelerated Aging Test Modeling for Polycarbonate: Effects of Light SourceMacromolecular Symposia, 2022
- Thermo-oxidative aging of the polyoxymethylene (POM), acrylonitrile–butadiene–styrene (ABS) and polycarbonate (PC) polymers – a comparative studyJournal of Polymer Research, 2022
- Effect of Low-Cycle Fatigue and Hydrothermal Aging on Tensile Properties of Open-Hole Glass Fiber/Polycarbonate and Glass Fiber/Polyamide 6 CompositesFibers and Polymers, 2021
- UV Aging Effects on Polycarbonate PropertiesJournal of Failure Analysis and Prevention, 2020
- Degradation of Polycarbonate Properties Under Thermal AgingJournal of Failure Analysis and Prevention, 2019
- Long term ageing of polyamide 6 and polyamide 6 reinforced with 30% of glass fibers: temperature effectJournal of Polymer Research, 2018
- Aging induced ductile-brittle-ductile transition in bisphenol A polycarbonateJournal of Polymer Research, 2018
- Durability of Glass Fibre Reinforced Polymer Pultruded Profiles: Comparison Between QUV Accelerated Exposure and Natural Weathering in a Mediterranean ClimateExperimental Techniques, 2016
- Study on the changing regularity of structure and properties of PC aged outdoor in western areas of ChinaJournal of Applied Polymer Science, 2012