Resistance to bond degradation between dual-cure resin cements and pre-treated sintered CAD-CAM dental ceramics
Open Access
- 1 January 2012
- journal article
- Published by Medicina Oral, S.L. in Medicina Oral Patología Oral y Cirugia Bucal
- Vol. 17 (4) , e669-e677
Abstract
Objective: To evaluate the bond stability of resin cements when luted to glass-reinforced alumina and zirconia CAD/CAM dental ceramics. Study design: Eighteen glass-infiltrated alumina and eighteen densely sintered zirconia blocks were randomly conditioned as follows: Group 1: No treatment; Group 2: Sandblasting (125 µm Al2O3-particles); and Group 3: Silica-coating (50 µm silica-modified Al2O3-particles). Composite samples were randomly bonded to the pre-treated ceramic surfaces using different resin cements: Subgroup 1: Clearfil Esthetic Cement (CEC); Subgroup 2: RelyX Unicem (RXU); and Subgroup 3: Calibra (CAL). After 24 h, bonded specimens were cut into 1 ± 0.1 mm2 sticks. One-half of the beams were tested for microtensile bond strength (MTBS). The remaining one-half was immersed in 10 % NaOCl aqueous solution (NaOClaq) for 5 h before testing. The fracture pattern and morphology of the debonded surfaces were assessed with a field emission gun scanning electron microscope (FEG-SEM). A multiple ANOVA was conducted to analyze the contributions of ceramic composition, surface treatment, resin cement type, and chemical challenging to MTBS. The Tukey test was run for multiple comparisons (p < 0.05). Results: After 24 h, CEC luted to pre-treated zirconia achieved the highest MTBS. Using RXU, alumina and zirconia registered comparable MTBS. CAL failed prematurely, except when luted to sandblasted zirconia. After NaOClaq storage, CEC significantly lowered MTBS when luted to zirconia or alumina. RXU decreased MTBS only when bonded to silica-coated alumina. CAL recorded 100 % of pre-testing failures. Micromorphological alterations were evident after NaOClaq immersion. Conclusions: Resin-ceramic interfacial longevity depended on cement selection rather than on surface pre-treatments. The MDP-containing and the self-adhesive resin cements were both suitable for luting CAD/CAM ceramics. Despite both cements being prone to degradation, RXU luted to zirconia or untreated or sandblasted alumina showed the most stable interfaces. CAL experimented spontaneous debonding in all tested groups.Keywords
This publication has 30 references indexed in Scilit:
- Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramicsDental Materials, 2009
- Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramicDental Materials, 2009
- Influence of saliva contamination on zirconia ceramic bondingDental Materials, 2008
- Microleakage in full-crown all-ceramic restorations: influence of internal surface treatment, silane application, alumina system, and substrate.2007
- Microtensile bond strength of a resin cement to silica-coated and silanized In-Ceram Zirconia before and after aging.2007
- Microtensile bond strength of a resin cement to glass infiltrated zirconia-reinforced ceramic: The effect of surface conditioningDental Materials, 2006
- Bonding of Resin Composite Luting Cements to Zirconium Oxide by Two Air-particle Abrasion MethodsOperative Dentistry, 2006
- The effect of silica coating on the resin bond to the intaglio surface of Procera AllCeram restorations.2003
- In vitro evaluation of long-term bonding of Procera AllCeram alumina restorations with a modified resin luting agentThe Journal of Prosthetic Dentistry, 2003
- Are adhesive technologies needed to support ceramics? An assessment of the current evidence.2002