Beta response of LiMgPO4:Tb,B based OSL discs for personnel monitoring applications

Authors:

Abstract
Properties such as high optically stimulated luminescent (OSL) sensitivity, ease of preparation and dose linearity over nine decades (µGy-kGy) make LiMgPO4:Tb, B (LMP) a unique phosphor for dosimetry applications. This led to the investigation of the beta response of highly sensitive LMP-based Teflon-embedded OSL discs for personnel monitoring applications. A PTB beta secondary standard calibration setup (BSS2), which contains three beta sources viz.147Pm, 85Kr and 90Sr/90Y, was used. The relative response with respect to 137Cs photons for 0.4-mm thick LMP discs was found to be ∼7.32, ∼53.5 and 100 % for 147Pm, 85Kr and 90Sr/90Y beta energies, respectively. The response of LMP discs under various filter combinations viz. 0.18-mm thick mylar (25 mg cm−2), 0.625-mm thick Poly-allyl-diglycol carbonate (PADC, 81 mg cm−2), 1-mm thick polythene (95 mg cm−2), 1-mm thick Perspex (118 mg cm−2), 1.25-mm thick PADC (162 mg cm−2) and 1.6-mm thick (189 mg cm−2) Perspex filters was also studied and the ratio of the response of open disc to the response under filters (DOpen/DFilter) of different thicknesses (mg cm−2) was evaluated. Studies were also performed for the mixed field of low- (85Kr) and high-energy (90Sr/90Y) beta particles and the DOpen/DFilter ratio was evaluated. The angular dependence of the response of OSL discs to 85Kr and 90Sr/90Y beta sources was also studied. Studies were also carried out for 204Tl, 32P, natural uranium and 106Ru/106Rh beta sources and the ratios of the response of open disc to that of under 1.6-mm thick Perspex (DOpen/DFilter) filter were measured. A study with various beta sources for the evaluation of the DOpen/DFilter ratio was necessary as these ratios are used to estimate the energy of beta particles and to apply the correction factor while evaluating the beta dose/design of dose estimation algorithms.

This publication has 12 references indexed in Scilit: