Effect of Different Liners on Fracture Resistance of Premolars Restored with Conventional and Short Fiber‐Reinforced Composite Resins
- 11 January 2018
- journal article
- research article
- Published by Wiley in Journal of Prosthodontics
- Vol. 28 (1) , e304-e309
Abstract
Purpose To see whether applying four different liners under short fiber-reinforced composite (SFRC), everX Posterior, compared to conventional composite resin, Z250, affected their strengthening property in premolar MOD cavities. Materials and Methods Mesio-occluso-distal (MOD) cavities were prepared in 120 sound maxillary premolars divided into 10 groups (n = 12) in terms of two composite resin types and 4 liners or no liner. For each composite resin, in 5 groups no liner, resin-modified glass ionomer (RMGI), conventional flowable composite (COFL), self-adhesive flowable composite resin (SAFL), and self-adhesive resin cement (SARC) were applied prior to restoring incrementally. After water storage and thermocycling, static fracture resistance was tested. Data (in Newtons) were analyzed using two-way ANOVA (α = 0.05). Results Fracture resistance was significantly affected by composite resin type (p = 0.02), but not by the liner (p > 0.05). The interaction of the two factors was not statistically significant (p > 0.05). SFRC exhibited higher fracture strength (1470 ± 200 N) compared to conventional composite resin (1350 ± 290), irrespective of the application of liners. Application of SARC and SAFL liners led to a higher number of restorable fractures for both composite resins. Conclusions The four liners can be used without interfering with the higher efficacy of SFRC, compared to conventional composite resins, to improve the fracture strength of premolar MOD cavities.Keywords
Funding Information
- Shiraz University of Medical Sciences (8261)
This publication has 35 references indexed in Scilit:
- 22-Year clinical evaluation of the performance of two posterior composites with different filler characteristicsDental Materials, 2011
- Fracture Resistance of Cuspal Coverage of Endodontically Treated Maxillary Premolars with Combined Composite-Amalgam Compared to Other TechniquesOperative Dentistry, 2011
- Effect of Conventional and Resin-modified Glass-Ionomer Liner on Dentin Adhesive Interface of Class I Cavity Walls After ThermocyclingOperative Dentistry, 2011
- Spatially resolved assessments of composite shrinkage in MOD restorations using a digital-image-correlation techniqueDental Materials, 2011
- Microleakage of Posterior Composite Restorations Lined with Self-adhesive Resin CementsOperative Dentistry, 2010
- Effect of low-elastic modulus liner and base as stress-absorbing layer in composite resin restorationsDental Materials, 2010
- Flowability of composites is no guarantee for contraction stress reductionDental Materials, 2009
- Polymerization shrinkage of experimental short glass fiber-reinforced composite with semi-inter penetrating polymer network matrixDental Materials, 2008
- Short glass fiber reinforced restorative composite resin with semi-inter penetrating polymer network matrixDental Materials, 2007
- Cuspal deflection and microleakage in premolar teeth restored with resin-based composites with and without an intermediary flowable layerJournal of Dentistry, 2007