Effects of temperature and humidity on high-strength p-aramid fibers used in body armor
Open Access
- 14 April 2020
- journal article
- research article
- Published by SAGE Publications in Textile Research Journal
- Vol. 90 (21-22) , 2428-2440
Abstract
To improve the reliability and design of body armor, it is imperative to understand the failure modes and the degradation rates of the materials used in armor. Despite the best efforts of manufacturers, some vulnerability of armor materials to aging due to hydrolytic or oxidative environments is expected and may result in the degradation of material properties such as tensile strength. In this work, p-aramid yarns from two manufacturers were exposed to environmental conditions of various fixed temperature and humidity combinations. The maximum temperature and humidity condition was 70℃ and 76% relative humidity (RH). Tensile tests were performed on specimens extracted at several different times over the course of at least 1 year to determine the change in ultimate tensile strength and failure strain as a function of time, temperature, and humidity. Molecular spectroscopy was used to investigate any chemical changes as a result of the aging. The p-aramid materials were found to be generally resistant to degradation at most conditions, showing changes of less than 10% only at the highest temperature and humidity conditions.Keywords
Funding Information
- National Institute of Standards and Technology (70NANB14H270, 70NANB17H337, 70NANB18H049, 70NANB18H222)
This publication has 33 references indexed in Scilit:
- Degradation of aramid fibers under alkaline and neutral conditions: Relations between the chemical characteristics and mechanical propertiesJournal of Applied Polymer Science, 2010
- Accelerated UV weathering device based on integrating sphere technologyReview of Scientific Instruments, 2004
- Influence of Hydrolytic and Chemical Treatment on the Mechanical Properties of Aramid and Copolyaramid FibersTextile Research Journal, 1998
- Moisture sorption mechanism of aromatic polyamide fibers. V: Growth of crystallites in as-spun wet poly(p-phenylene terephthalamide) fiber during dehydrationJournal of Polymer Science Part B: Polymer Physics, 1997
- Moisture sorption mechanism of aromatic polyamide fibres: diffusion of moisture into regular Kevlar as observed by time-resolved small-angle X-ray scattering techniquePolymer, 1994
- Quantitative characterization of spectral ultraviolet radiation-induced photodegradation in coating systems exposed in the laboratory and the fieldProgress in Organic Coatings, 1993
- Studies in accelerated weatheringProgress in Organic Coatings, 1991
- Kinetics for the tensile strength degradation of nylon and kevlar yarnsJournal of Applied Polymer Science, 1989
- Surface Studies of Polymer Films and Fibers by CIRCLE ATR FT-IRApplied Spectroscopy, 1988