Fracture strength of two oxide ceramic crown systems after cyclic pre‐loading and thermocycling
- 8 August 2006
- journal article
- research article
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 33 (9) , 682-689
Abstract
The aim of the present study was to investigate the fracture resistance of zirconia crowns and to compare the results with crowns made of a material with known clinical performance (alumina) in away that reflects clinical aspects. Sixty crowns were made, 30 identical crowns of alumina and 30 of zirconia. Each group of 30 was randomly divided into three groups of 10 crowns that were to undergo different treatments: (i) water storage only, (ii) pre-loading (10 000 cycles, 30-300 N, 1 Hz), (iii) thermocycling (5-55 degrees , 5000 cycles) + pre-loading (10 000 cycles, 30-300 N, 1 Hz). Subsequently, all 60 crowns were subjected to load until fracture occurred. There were two types of fracture: total fracture and partial fracture. Fracture strengths (N) were: group 1, alumina 905/zirconia 975 (P = 0.38); group 2, alumina 904/zirconia 1108 (P < 0.007) and group 3, alumina 917/zirconia 910 (P > 0.05). Total fractures were more frequent in the alumina group (P < 0.01). Within the limitations of this in vitro study, it can be concluded that there is no difference in fracture strength between crowns made with zirconia cores compared with those made of alumina if they are subjected to load without any cyclic pre-load or thermocycling. There is, however, a significant difference (P = 0.01) in the fracture mode, suggesting that the zirconia core is stronger than the alumina core. Crowns made with zirconia cores have significantly higher fracture strengths after pre-loading.Keywords
This publication has 15 references indexed in Scilit:
- All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical studyJournal of Oral Rehabilitation, 2005
- Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramicsDental Materials, 2004
- In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cyclingThe Journal of Prosthetic Dentistry, 2004
- Tooth preparations for complete crowns: An art form based on scientific principlesThe Journal of Prosthetic Dentistry, 2001
- Lifetime-limiting Strength Degradation from Contact Fatigue in Dental CeramicsJournal of Dental Research, 2000
- Predicting lifetimes of materials and material structuresDental Materials, 1995
- Perspectives on strengthDental Materials, 1995
- Mechanical properties and short‐term in vivo evaluation of yttrium‐oxide‐partially‐stabilized zirconiaJournal of Biomedical Materials Research, 1989
- Structural ceramics: A question of fabrication reliabilityJournal of Materials for Energy Systems, 1984
- Influence of Reaction Products on Reaction Between Water and Soda‐Lime‐Silica GlassJournal of the American Ceramic Society, 1958