Characterization of polyisobutylene‐based model urethane networks

Authors:

Abstract
Polyisobutylene‐based model urethane networks have been prepared by crosslinking liquid α, ω‐di(hydroxyl)polyisobutylenes, i.e., PIB‐diols carrying exactly two CH2OH functions, Fn = 2.0 ± 0.1, and rather narrow molecular weight distributions, Mw/Mn = 1.5−1.6, with tritriphenylmethyl isocyanate \documentclass{article}\pagestyle{empty}$$\rm{HC}\ (\hskip-6pt\hbox{---}p\rm{C}_6\rm{H}_4\hbox{---}\rm{NCO})_3$$ . Networks prepared with Mn = 1400 and 7500 PIB‐diols, and with 90/10 and 80/20 mixtures of these PIB‐diols (bimodal networks), have been characterized by extraction, by the Flory–Rehner swelling method, and by the Mooney–Rivlin equilibrium modulus method, and tested by stress–strain measurements. Mc values of the Mn = 1400 PIB‐diol network obtained by swelling (1550) and by equilibrium modulus studies (1500) were in excellent agreement with the Mn of the prepolymer. Also the C2 parameter was negligible in comparison to C1, suggesting the absence of interchain entanglements. This is the first hydrocarbon‐based polyurethane network that exhibits a negligible C2 value by stress–strain measurements of unswollen samples. The Mc values of the Mn = 7500 PIB‐diol were also in good agreement with the Mn of the prepolymer; however, C2 was larger than C1, indicating interchain entanglements. Evidence for strain‐induced toughening was observed with both networks prepared with the Mn = 1400 and 7500 PIB‐diols. The ultimate properties of the two bimodal networks did not show improvement over those of the individual constituents; however, the Mn's of the constituents were not very different.

This publication has 18 references indexed in Scilit: