Effects of layer thickness and alloy composition on carrier lifetimes in mid-wave infrared InAs/InAsSb superlattices

Authors:

Abstract
Measurements of carrier recombination rates using a time-resolved pump-probe technique are reported for mid-wave infrared InAs/InAs1−xSbx type-2 superlattices (T2SLs). By engineering the layer widths and alloy compositions, a 16 K band-gap of ≃235 ± 10 meV was achieved for all five unintentionally doped T2SLs. Carrier lifetimes were determined by fitting a rate equation model to the density dependent data. Minority carrier lifetimes as long as 10 μs were measured. On the other hand, the Auger rates for all the InAs/InAsSb T2SLs were significantly larger than those previously measured for InAs/GaSb T2SLs. The minority carrier and Auger lifetimes were observed to generally increase with increasing antimony content and decreasing layer thickness.
Funding Information
  • U.S. Department of Energy (DE-AC04-94AL85000)

This publication has 28 references indexed in Scilit: