Tribological properties of bronze–Cr–Ag alloy in seawater, NaCl solution and deionized water
Authors:
- Kongjie JinKJKongjie Jin
- Zhuhui QiaoZQZhuhui Qiao
- Shengyu ZhuSZShengyu Zhu
- Jun ChengJCJun Cheng
- Bing YinBYBing Yin
- Jun YangJYJun Yang
- 1 June 2016
- journal article
- Published by Elsevier in Tribology International
- Vol. 98, 1-9
Abstract
No abstract availableKeywords
Funding Information
- National Natural Science Foundation of China (51227804, 51303188)
- Changchun Institute of Applied Chemistry, Chinese Academy of Sciences (RERU2014008)
This publication has 59 references indexed in Scilit:
- In situ Raman spectroscopy study of corrosion products on the surface of carbon steel in solution containing Cl− and
SO
4
2
-
Engineering Failure Analysis, 2011
- Tribological properties of Fe3Al material under water environmentMaterials Science and Engineering: A, 2008
- Fatigue of highly strengthened Cu–Ag alloysInternational Journal of Fatigue, 2008
- The influence of nickel–aluminium bronze microstructure and crevice solution on the initiation of crevice corrosionElectrochimica Acta, 2008
- The Solution Structure of [Cu(aq)]2+ and Its Implications for Rack-Induced Bonding in Blue Copper Protein Active SitesInorganic Chemistry, 2007
- Microstructure and properties of a Cu–Cr–Zr alloyJournal of Nuclear Materials, 2001
- Complexation of Cu2+ in oxidized NaCl brines from 25°C to 175°C: results from in situ EXAFS spectroscopyChemical Geology, 2000
- Solubility in the CuCl2-NaCl-H2O System and Hydration Analysis in the Case of ComplexationCollection of Czechoslovak Chemical Communications, 1999
- Intercomparison of surface analysis of thin aluminium oxide filmsSurface and Interface Analysis, 1990
- X-ray photoelectron spectroscopy studies of solvated metal atom dispersed catalysts. Monometallic iron and bimetallic iron-cobalt particles on aluminaChemistry of Materials, 1990