Corrosion resistance of nickel coatings deposited from low-temperature nickel-plating electrolytes
- 1 April 2017
- journal article
- Published by Pleiades Publishing Ltd in Russian Journal of Applied Chemistry
- Vol. 90 (4) , 566-573
Abstract
The corrosion resistance of nickel coatings on a copper substrate, plated from low-temperature electrolytes based on acetates, tartrates, and isobutyrates, was studied by the methods of electrochemical impedance spectroscopy (EIS) and polarization curves. The tests were performed in a 0.3% NaCl solution. The nickel coatings exhibit high chemical activity, dissolving in the NaCl solution. The electrochemical step is the limiting step of the corrosion process.Keywords
This publication has 11 references indexed in Scilit:
- Effect of current density on wettability and corrosion resistance of superhydrophobic nickel coating deposited on low carbon steelMaterials & Design, 2017
- An investigation on the effect of surface morphology and crystalline texture on corrosion behavior, structural and magnetic properties of electrodeposited nanocrystalline nickel filmsApplied Surface Science, 2014
- Nickel electrocrystallization in different electrolytes: An in-process and post synthesis analysisElectrochimica Acta, 2013
- Effect of gluconate addition on the electrodeposition of nickel from acidic bathsSurface and Coatings Technology, 2012
- Effect of grain size on corrosion behavior of electrodeposited bulk nanocrystalline NiTransactions of Nonferrous Metals Society of China, 2010
- Electroplating of catalytically active nickel coatings from baths of various anionic compositionsProtection of Metals and Physical Chemistry of Surfaces, 2009
- Corrosion resistance and mechanical properties of pulse electrodeposited Ni–TiO2 composite coating for sintered NdFeB magnetJournal of Alloys and Compounds, 2009
- Nickel electrodeposition from novel citrate bathTransactions of Nonferrous Metals Society of China, 2007
- Bright nickel plating from nickel citrate electroplating bathsMetal Finishing, 2004
- The electrochemical deposition of nickel from electrolytes containing malonic acidSurface and Coatings Technology, 2002