Abstract
We have studied the electronic structure of Co ions in semiconducting anatase Co:TiO2(1.4 at.% Co) with x-ray-absorption spectroscopy. The density of structural defects is varied by (i) the oxygen vacancy concentration depending on the oxygen background pressure during growth, and (ii) the film thickness. The Co L2,3-edge spectra, which are characteristic of Co2+ (3d7) ions, show particularly pronounced ligand-to-metal charge-transfer (CT) satellites for the thickest oxygen-poor films, which also exhibit the highest structural defect density. With charge-transfer multiplet calculations, the CT satellites are modeled by configuration interaction, originating from hybridization between Co 3d- and ligand states. This hybridization adds to the complex interplay between Co heterogeneity, defects, and electronic and magnetic properties in Co:TiO2. DOI: http://dx.doi.org/10.1103/PhysRevB.83.134404 ©2011 American Physical Society

This publication has 28 references indexed in Scilit: