Synthesis of a pyrrolone‐type polymer containing anthraquinone units in molten antimony trichloride

Authors:

Abstract
1,2,5,6‐Tetraaminoanthraquinone and 1,4,5,8‐naphthalenetetracarboxylic acid dianhydride react in molten antimony trichloride to give a soluble polypyrrolone structure with an inherent viscosity of 0.4–0.7. Polymers having the viscosity of 0.7 can be wetspun into fibers from molten antimony trichloride or from methanesulfonic acid; also the polymer can be reduced with sodium dithionite in alkaline aqueous dimethyl sulfoxide to give a viscous solution which can be spun into brittle fibers.