Temperature and rate dependent debonding behaviors of precision glass molding interface
- 21 September 2020
- journal article
- research article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 104 (1) , 243-255
Abstract
The glass‐to‐mold adhesion in precision glass molding could severely degrade the quality of molded optics and shorten the lifespan of the precious molds. Since the consequences of adhesion take effect during the separation between glass and molds, it is important to investigate the debonding behaviors of a typical glass molding interface. To this end, here we perform a probe tack test procedure for borosilicate glass BK7, where debonding is conducted at molding temperature and specific velocity. We fully characterize the debonding behaviors using the peak adhesion stress σ max and the work of debonding W deb . Experiments show that when temperature is decreased from 690°C to 655°C at 10 μm/s, σ max continuously increases, while W deb first increases but then sharply decreases. When the debonding velocity is increased from 10 to 50 μm/s at 680°C, σ max also increases while W deb overall decreases. Therefore, the debonding behaviors are highly temperature and rate dependent. More importantly, depending on the debonding conditions, three debonding types are identified, that is, the cohesive bulk deformation, the cohesive‐interfacial transition and the interfacial fracture. The cohesive type can be converted into the interfacial fracture, by either decreasing temperature or increasing the debonding velocity. Based on the W deb criterion, the three debonding regimes can be clearly distinguished. Finally, analyses on the temperature and velocity experimental results are unified by incorporating the reduced crack velocity a T v c . The dependences of both viscoelasticity and W deb on a T v c qualitatively explain the transition condition for different debonding types. Concerning these findings, the work of debonding not only supplements the characterization of adhesion strength, but also throws insightful light on revealing the debonding mechanisms.Keywords
Funding Information
- Natural Science Foundation of Anhui Province (1808085ME118)
- National Natural Science Foundation of China (51905141, 51975174)
This publication has 33 references indexed in Scilit:
- PtIr protective coating system for precision glass molding tools: Design, evaluation and mechanism of degradationSurface and Coatings Technology, 2020
- High quality anti-sticking coating based on multilayer structureSurface and Coatings Technology, 2019
- Atomic diffusion induced degradation in bimetallic layer coated cemented tungsten carbideCorrosion Science, 2017
- Model of coating wear degradation in precision glass moldingThe International Journal of Advanced Manufacturing Technology, 2016
- Evaluation of demolding force for glass-imprint processJournal of Non-Crystalline Solids, 2014
- Graphene-coated Si mold for precision glass optics moldingOptics Letters, 2013
- Determination of adhesive forces and sticking temperature of coated glasses for the hot-embossing-processMicrosystem Technologies, 2011
- Investigation of the effects of process parameters on the glass-to-mold sticking force during precision glass moldingSurface and Coatings Technology, 2010
- Wetting, interfacial interactions and sticking in glass/steel systemsMaterials Science and Engineering: A, 2004
- A study on separation behavior of press‐molded glassware from a thermal engineering viewpoint: Correlation of separation forces to the interface temperature between the mold and the glassHeat Transfer, 2001