The Effect of Nano-Silica Surface Infiltration on Bond Strength of a Phosphate-Monomer-containing Composite Cement to Zirconia
Authors:
Open Access
- 1 January 2023
- journal article
- research article
- Vol. 25 (1) , 79-86
Abstract
Purpose: To evaluate the bonding receptiveness of zirconia treated with nano-silica surface infiltration and the bond strength of composite cement after aging. Materials and Methods: Zirconia ceramic green bodies (Ceramill zolid, Amann Girbach) with dimensions of 10 x 10 x 4 mm were divided into three groups (n = 4): group C (control: no treatment after sintering), group S (sandblasted: 50-mu m alumina airborne particle abrasion after sintering) and group N (nanosintered: infiltrated with nano-silica colloid, sintered, and then etched with hydrofluoric acid). Phase transformations were examined through X-ray diffraction (XRD). Composite resin (Filtek Z250, 3M Oral Care) was bonded to zirconia using the 10-MDP-containing composite cement Panavia F (Kuraray Noritake). The composite-cement/ zirconia bond strength was immediately measured using the microtensile bond strength test (mu TBS) as well as after three months of artificial aging in water (n = 20 microstick specimens/group). Failure mode patterns were examined using SEM. Results: The specimens of groups C and S, as tested by XRD, exhibited almost full tetragonal phases, while a small extent of tetragonal-monoclinic phase transformation (t -> m) was observed for group N. Group N achieved the highest bond strengths (41.5 +/- 8.6 MPa), which was significantly higher than that measured for groups C and S (p < 0.05). There was a significant drop in mu TBS after 90 days of water storage for groups C and S. SEM revealed a decrease in the percentage of cohesive failure in groups N and S after water storage. Conclusions: Infiltrating zirconia with nano-silica is a reliable method to establish a strong and stable bond to zirconia. The combination of surface infiltration with nano-silica and application of a phosphate monomer-containing composite cement can significantly improve the composite-cement/zirconia bond strength.Keywords
This publication has 55 references indexed in Scilit:
- The effect of preparation order on the crystal structure of yttria-stabilized tetragonal zirconia polycrystal and the shear bond strength of dental resin cementsDental Materials, 2011
- Innovations in bonding to zirconia based ceramics: Part III. Phosphate monomer resin cementsDental Materials, 2010
- Bonding to Zirconia Using a New Surface TreatmentJournal of Prosthodontics, 2010
- Influence of different surface treatments on surface zirconia frameworksJournal of Dentistry, 2009
- Surface modification for enhanced silanation of zirconia ceramicsDental Materials, 2009
- Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramicDental Materials, 2009
- All-ceramic inlay-retained fixed partial dentures: Preliminary results from a clinical studyJournal of Dentistry, 2008
- Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditionsDental Materials, 2007
- Microtensile bond strength of different components of core veneered all-ceramic restorationsDental Materials, 2006
- Failure analysis of resin composite bonded to ceramicDental Materials, 2003