Abstract
With the addition of 1 wt% of MgO–Al2O3–SiO2 glass as a sintering aid, 3Y‐TZP/12Ce‐TZP ceramics (composed from a mixture of 3Y‐TZP and 12Ce‐TZP powder) have been fabricated via liquid‐phase sintering at 1250°–1400°C. In the sintered bodies, the grain growth of Y‐TZP is almost unaffected, whereas that of Ce‐TZP is inhibited. MgO·Al2O3 spinel and an amorphous phase that contains Al2O3 and SiO2 (from the sintering aid) fully fill the grain junctions. The bending strength of 3Y‐TZP/12Ce‐TZP, when sintered at 1250°–1300°C, is ∼800–900 MPa, which is greater than that of 3Y‐TZP ceramics without Ce‐TZP particles. Ce‐TZP grains and MgO·Al2O3 spinel in 3Y‐TZP/12Ce‐TZP ceramics may impede crack growth, and the bending strength is enhanced.