Abstract
We report the synthesis of CuO material by molten salt method at a temperature range, 280 to 950 °C for 3 h in air. This report includes studies on the effect of morphology, crystal structure and electrochemical properties of CuO prepared at different temperatures. Obtained CuO was characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), and Brunauer–Emmett–Teller (BET) surface area methods. Samples prepared at ≥410 °C showed a single-phase material with a lattice parameter value of a = 4.69 Å, b = 3.43 Å, c = 5.13 Å and surface area values are in the range 1.0–17.0 m2 g–1. Electrochemical properties were evaluated via cyclic voltammetry (CV) and galvanostatic cycling studies. CV studies showed a minor difference in the peak potentials depending on preparation temperature and all compounds exhibit a main anodic peak at ∼2.45 V and cathodic peaks at ∼0.85 V and ∼1.25 V vs Li. CuO prepared at 750 °C showed high and stable capacity of ∼620 mA h g–1 at the end of 40th cycle.