Subsea Dissimilar Joints: Failure Mechanisms and Opportunities for Mitigation
Authors:
- 22 March 2009
- conference paper
- Published by Association for Materials Protection and Performance (AMPP)
- p. 1-12
Abstract
Dissimilar joints are a common part of subsea oil and gas systems where clad forged fittings are joined to clad or CRA pipe. Whilst the majority of these joints have given successful service, a small number have failed. In the current work, environmental testing was carried out on a dissimilar joint to an 8630M forging, buttered using alloy 625. Tests were monitored using a sensitive technique in order to capture the first moments of crack initiation and to determine the minimum threshold stress intensity factor Kth, below which there is no environmentally assisted cracking. Two distinct initiation mechanisms were identified; one dependent on hydrogen-charging in service (under cathodic protection) and one not. A detailed microstructural investigation, including chemistry, structure and strain, gave insight into the attributes of the ‘partially mixed zone’ (PMZ) immediately adjacent to the fusion boundary, on the weld side, in which one of the failure modes occurred. The chemical and microstructural characteristic of this PMZ are influenced by welding and postweld heat treatment (PWHT) parameters. Based on this investigation, the potential for mitigation of cracking susceptibility by materials selection or by modifying the welding/PWHT procedure is discussed.Keywords
This publication has 3 references indexed in Scilit:
- Carbon paraequilibrium in austenitic stainless steelMetallurgical and Materials Transactions A, 2006
- Segregation Effects and Phase Developments during Solidification of Alloy 625Materials Science Forum, 2006
- Colossal carbon supersaturation in austenitic stainless steels carburized at low temperatureActa Materialia, 2003