Hydrogen Embrittlement of PH13–8Mo Steel in Simulated Real-Life Tests and Slow Strain Rate Tests
Authors:
- 1 April 1990
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 46 (4) , 286-295
Abstract
The environmentally assisted cracking or hydrogen embrittlement (HE) of a precipitation-hardening stainfess steel, PH13–8Mo (UNS(1) S13800), has been investigated by simulated real-life testing and accelerated slow strain rate testing (SSRT). The simulated real-life tests involved alternate immersion in 3.5% NaCl of notched specimens galvanically coupled to aluminum, while in the SSRT smooth specimens were galvanostatically charged with hydrogen. In both cases, specimens were tested in an underaged, a peak-aged, and an overaged condition. The findings for both tests show that the susceptibility of the steel to hydrogen embrittlement decreases as the aging temperature is increased. This means that the susceptibility is not dependent solely on strength but must be related to microstructural variations. This is discussed with reference to transmission electron microscopy (TEM) micrographs. In addition to the above tests, elastic slow strain rate tests, in which the specimens are prestrained in air before restraining while charging with hydrogen, were carried out to investigate the role of plastic straining in crack initiation.Keywords
This publication has 5 references indexed in Scilit:
- Hydrogen Embrittlement of PH 13-8 Mo Stainless Steel—The Effect of Surface ConditionCorrosion, 1984
- Precipitation hardening in a PH 13-8 Mo stainless steelMaterials Science and Engineering, 1981
- Stress-Corrosion Cracking Evaluation of Aerospace Bolting Alloys1976
- Stress-Corrosion Cracking Properties of 17-4 PH Steel1976
- Stress Corrosion Properties of High Strength Precipitation Hardening Stainless SteelsCorrosion, 1971