Abstract
The Sillenite type Bi24B2O39 is an incongruently melting compound at Tp = 650 °C. Single crystals have been grown from non‐stoichiometric melts as well as from high temperature solutions by the Czochralski method and by a top seeded solution growth technique (TSSG), respectively.The main difficulty in the crystal growth of Bi24B2O39 arises from the very small field of crystallization in the binary system Bi2O3–B2O3. Further problems are caused by the nearly simultaneous formation of the 2:1 compound Bi4B2O9 and the 12:1 compound Bi24B2O39. Therefore, a precise thermal reinvestigation of the phase diagram was carried out using DTA‐technique on the Bi2O3‐rich side. Additionally, crystal growth runs have been started in the ternary system Bi2O3–B2O3–Li2O in order to extend the crystallization field. Homogeneous melts were more difficult to prepare because of the high density difference between Bi2O3 (∂ = 9.3 g/cm3) and B2O3 (∂ = 2.46 g/cm3). The homogeneity of the melts were improved, using Bi2O3 and synthesized Bi4B2O9 (∂ = 8.25 g/cm3) as starting materials. As a result of this procedure, small crystals of Bi24B2O39 were grown from these starting materials and the lattice parameter were determined.

This publication has 2 references indexed in Scilit: