Critical Role of the Crystallite Size in Nanostructured Li4Ti5O12 Anodes for Lithium-Ion Batteries

Authors:

Abstract
Lithium titanate Li4Ti5O12 (LTO) is regarded as a promising alternative to carbon-based anodes in lithium-ion batteries. Despite its stable structural framework, LTO exhibits disadvantages such as the sluggish lithium-ion diffusion and poor electronic conductivity. In order to modify the performance of LTO as an anode material, nanosizing constitutes a promising approach, and the impact is studied here by systematical experimental approach. Phase-pure polycrystalline LTO nanoparticles (NPs) with high crystallinity and crystallite sizes ranging from 4 to 12 nm are prepared by an optimized solvothermal protocol and characterized by several state-of-the-art technologies including HRTEM, XRD, PDF (pair distribution function) analysis, Raman spectroscopy and XPS. Through a wide array of electrochemical analyses, including charge/discharge profiles, cyclic voltammetry (CV) and electrochemical impedance spectroscopy (EIS), a crystallite size of approx. 7 nm is identified as optimum particle size. Such NPs exhibit as good reversible capacity as the ones with larger crystallite sizes, but a more pronounced interfacial charge storage. By decreasing the crystallite size to about 4 nm the interfacial charge storage increases remarkably, however resulting in a loss of reversible capacity. An in-depth structural characterization using the PDF obtained from synchrotron XRD data indicates an enrichment in Ti for NPs with the small crystallite sizes, and this Ti-rich structure enables a higher Li storage. The electrochemical characterization confirms this result and furthermore points to a plausible reason why a higher Li-storage in very small nanoparticles (4 nm) results in a loss in the reversible capacity.
Funding Information
  • China Scholarship Council (2011631008)
  • Federal State of Hessen

This publication has 57 references indexed in Scilit: