Effect of Mode of Application on the Microtensile Bond Strength of a Self-etch and Etch-and-Rinse Adhesive System
Authors:
- A. ReisARA. Reis
- C. Zander-GrandeCZC. Zander-Grande
- S. KossatzSKS. Kossatz
- R. StanislawczukRSR. Stanislawczuk
- A. MansoAMA. Manso
- R. M. CarvalhoRCR. M. Carvalho
- A. D. LoguercioALA. D. Loguercio
Open Access
- 1 July 2010
- journal article
- research article
- Published by Operative Dentistry in Operative Dentistry
- Vol. 35 (4) , 428-435
Abstract
All Bond 3 and All Bond Self-Etch are versatile systems, capable of being used either in the full or simplified version. Both showed adequate microtensile bond strength results in enamel and dentin after 24 hours of water storage. This study examined the 24-hour microtensile bond strength (μTBS) of a three-step etch-and-rinse (All Bond 3 [AB3]) and a two-step self-etch system (All Bond Self-Etch [ABSE]) to dentin and ground enamel, varying the application mode. Methods: AB3 was applied according to the following procedures:A–phosphoric acid + adhesive application. The adhesive was then light-cured before resin buildup. B–similar to Procedure A, except that a thin layer of bonding resin was applied over the cured adhesive; C–similar to Procedure B, however, the adhesive was not light-cured before application of the bonding resin. ABSE was applied according to the following procedures: A–the acidic adhesive was applied and light-cured; B–after the acidic adhesive application and light-curing, a thin layer of ABSE Liner was applied and light cured; C–similar to B, however, the acidic adhesive was not light cured before application of the ABSE Liner. Resin composite buildups (Charisma) were bonded to teeth substrates after adhesive application. The bonded specimens were sectioned into beams 0.9 mm2 after storage in water (24 hours/37°C) and subjected to μTBS with a crosshead speed of 0.5 mm/minute. The average values (MPa) obtained in each substrate were subjected to two-way repeated measures ANOVA and the Tukey's test (α=0.05). Results: No significant difference was observed among the experimental groups either in ground enamel or dentin. Conclusions: The 24-hour microtensile bond strength of All Bond 3 and All Bond Self-Etch was similar, regardless the mode of application of the adhesive systems.Keywords
This publication has 18 references indexed in Scilit:
- Effect of evaporation of primer components on ultimate tensile strengths of primer–adhesive mixtureDental Materials, 2005
- Effect of smear layer thickness and acidity of self-etching solutions on early and long-term bond strength to dentinJournal of Dentistry, 2005
- Four‐year water degradation of a resin‐modified glass‐ionomer adhesive bonded to dentinEuropean Journal of Oral Sciences, 2004
- Adhesive permeability affects coupling of resin cements that utilise self-etching primers to dentineJournal of Dentistry, 2004
- Single-step adhesives are permeable membranesJournal of Dentistry, 2002
- Effects of mechanical properties of adhesive resins on bond strength to dentinDental Materials, 2002
- Fractured surface characterization: wet versus dry bondingDental Materials, 2002
- In vivo Influence of Residual Moisture on Microtensile Bond Strengths of One‐Bottle AdhesivesJournal of Esthetic and Restorative Dentistry, 2002
- Adverse surface interactions between one-bottle light-cured adhesives and chemical-cured compositesDental Materials, 2001
- A Simple Method of Increasing the Adhesion of Acrylic Filling Materials to Enamel SurfacesJournal of Dental Research, 1955