(Ti,W)C-Based Ceramics: Processing, Microstructural Evolution, Strengthening Mechanisms, and Performance
Open Access
Abstract
The rapid development of advanced structural systems imposes increasingly severe thermomechanical demands on engineering materials operating under extreme service environments. Consequently, the development of high-performance structural materials capable of enduring such harsh conditions has become a primary research focus. Owing to their high melting points, elevated hardness, and thermodynamic stability, (Ti,W)C solid-solution ceramics have emerged as promising candidate materials for high-temperature and extreme-environment structural components. This review presents a systematic overview of recent advancements in (Ti,W)C-based ceramics across processing, microstructural, and performance domains. Specifically, the effects of consolidation techniques—including hot pressing (HP), spark plasma sintering (SPS), and reactive sintering (RS)—on densification kinetics, grain growth behavior, and core–rim microstructural evolution are critically discussed. Furthermore, the governing strengthening and toughening mechanisms, such as solid-solution strengthening, secondary-phase dispersion, and crack-tip shielding (predominantly crack deflection and bridging), are comprehensively examined, alongside their behavioral response and degradation-mitigation mechanisms under extreme service environments. Finally, current processing bottlenecks, brittleness issues, and manufacturing challenges are critically outlined, providing prospective research directions for the future development and engineering application of (Ti,W)C ceramics.Keywords
Funding Information
- National Natural Science Foundation of China (52002098)
- Heilongjiang Provincial Natural Science Foundation of China (LH2023E080)
- State Key Laboratory of Precision Welding & Joining of Materials and Structures (MSWJ-26M-09)
This publication has 110 references indexed in Scilit:
- Development of Ductile Refractory Alloys With Excellent High‐Temperature Strength for Extreme EnvironmentsAdvanced Materials, 2026
- Oxidation Behavior and Kinetics of (Ti,W)C-WSi2-SiC Composite at 1000-1100 °C: Role of Silicon in Protective Layer Formation and DegradationJournal of Materials Engineering and Performance, 2026
- Near‐Net‐Shaping of Ultra‐High Temperature Ceramics2014
- Effect of Mo2C on the Microstructure and Mechanical Properties of (Ti, W)C–Ni CermetsPowder Metallurgy and Metal Ceramics, 2014
- Ab initio study on fracture toughness of Ti0.75X0.25C ceramicsJournal of Materials Science, 2007
- Springer Handbook of Condensed Matter and Materials Data2005
- The Chemistry of Transition Metal Carbides and Nitrides1996
- Microstructure and mechanical properties of hot-pressed SiC-TiC compositesJournal of Materials Science, 1991
- Tailoring Multiphase and Composite Ceramics1986
- A Statistical Theory of Solid Solution HardeningPhysica Status Solidi (b), 1970