The response of SiC fibres to vacuum plasma spraying and vacuum hot pressing during the fabrication of titanium matrix composites
Authors:
- 1 November 1999
- journal article
- research article
- Published by Wiley in Journal of Microscopy
- Vol. 196 (2) , 162-174
Abstract
Vacuum plasma spraying (VPS) and vacuum hot pressing (VHP) have been used to fabricate Ti‐6Al‐4V matrix composite material reinforced longitudinally with DERA Sigma C coated SiC 1140+ fibres. VPS of Ti‐6Al‐4V onto Sigma 1140+ SiC fibres caused no fibre/matrix interfacial reaction. During VHP a fibre/matrix reaction occurred, producing a mixture of fine (< 50 nm) TiCx(x ≤ 1) adjacent to the fibre coating and coarse‐grained (0.3–0.5 μm) equiaxed TiCxadjacent to the Ti matrix. A decrease in C concentration with increasing distance from the C coating is proposed, and is consistent with the evidence presented. A similar thickness and morphology of reaction product arose from conventional foil–fibre foil processing, but the matrix coated fibre/hot isostatic pressing process led to a slightly thicker reaction layer. The TiCxreaction product acted as a diffusion barrier, inhibiting further reaction more effectively than in experiments on earlier SiC fibres having a C coating.Surface damage was shown to be a factor in lowering 1140+ SiC fibre failure stress. Surface damage to 1140+ fibres resulted from both VPS and VHP, the former causing a slight reduction in mean ultimate tensile strength (UTS), and a large reduction in the bend strain to failure Weibull modulus. This damage was caused by both fibre winding and by deposition of metal during VPS, giving rise to coating flaws, and is not in itself considered to be a major problem. Surface damage increased after VHP, reducing the mean UTS and tensile Weibull modulus, and the mean bend strain to failure. This damage arose from bending and flattening of the rough monotapes, and from the fibre/matrix reaction caused by thermal exposure. The level of damage to 1140+ SiC fibre from VHP was reduced by modification of the process path. Increasing the VHP temperature and lowering the pressure ramp rate reduced fibre damage sufficiently to enable a macroscopic composite UTS of 95% of the theoretical maximum to be achieved.Keywords
This publication has 29 references indexed in Scilit:
- Fibre-reinforced intermetallic compounds by physical vapour depositionMaterials Science and Engineering: A, 1995
- Spray Processing of Ti Metal Matrix Composites1995
- Solid-state fabrication and interfaces of fibre reinforced metal matrix compositesProgress in Materials Science, 1995
- Interface microstructures in Ti-based composites using TiB2/C-coated and uncoated SiCf after short-term thermal exposureComposites, 1994
- Evaluation of the efficiency of TiB2 and TiC as protective coatings for SiC monofilament in titanium-based compositesJournal of Materials Science, 1994
- Fabrication of advanced metal and intermetallic composite materials by the wire arc spray process —an extended abstractJournal of Thermal Spray Technology, 1994
- On the diffusion of carbon in titanium carbideMetallurgical Transactions A, 1989
- Ti-6Al-4V-2Ni as a matrix material for a SiC-reinforced compositeMetallurgical Transactions A, 1987
- Fibre-reinforced metal-matrix compositesComposites, 1985
- SiC filament/titanium matrix composites regarded as model compositesJournal of Materials Science, 1984