Tensile Creep and Creep‐Recovery Behavior of a SiC‐Fiber─Si 3 N 4 ‐Matrix Composite
Authors:
- 1 May 1993
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 76 (5) , 1281-1293
Abstract
The tensile creep and creep‐recovery behavior of a unidirectional SiC‐fiber/Si 3 N 4 ‐matrix composite was investigated at 1200°C in air. A primary objective of the study was to determine how various sustained and cyclic creep loading histories would influence the creep rate, accumulated creep strain, and the amount of strain recovered upon specimen unloading. The key results obtained from the investigation can be summarized as follows: (1) A threshold stress of 60 MPa was identified, below which the creep rate of the composite was exceedingly low (∼10 −12 s −1 ). (2) Periodic fiber fracture was identified as a fundamental damage mode for sustained tensile creep at stresses of 200 and 250 MPa. (3) Because of transient stress redistribution between the fibers and matrix, the creep life and failure mode at 250 MPa. were strongly influenced by the rate at which the initial creep stress was applied. (4) Very dramatic creep‐strain recovery occurred during cyclic creep; for cyclic loading between stress limits of 200 and 2 MPa, 80% of the prior creep strain was recovered during 50‐h‐creep/ 50‐h‐unloading cycles and over 90% during 300‐s‐creep/ 300‐s‐unloading cycles. (5) Cyclic loading significantly lowered the duration of primary creep and overall creep‐strain accumulation. The implications of the results for microstructural and component design are discussed.Keywords
This publication has 37 references indexed in Scilit:
- High‐Temperature Failure of an Alumina‐Silicon Carbide Composite under Cyclic loads: Mechanisms of Fatigue Crack‐Tip DamageJournal of the American Ceramic Society, 1989
- Tough Silicon Nitride Matrix Composites Using Textron Silicon Carbide Monofilaments1989
- Creep Behavior of an Al2O3-Sic CompositeMRS Proceedings, 1988
- The Mechanical Properties at High Temperatures of SiC Whisker-Reinforced AluminaMRS Proceedings, 1988
- Cyclic Fatigue of Hot-Pressed Si3N4sb>at High TemperaturesAdvanced Ceramic Materials, 1986
- Formation of LanxideTM ceramic composite materialsJournal of Materials Research, 1986
- Deformation Behavior of SiC Whisker Reinforced Si3N4MRS Proceedings, 1986
- Processing and Creep Performance of Silicon Carbide Whisker-Reinforced Silicon NitrideMRS Proceedings, 1986
- Silicon carbide fibre reinforced glass-ceramic matrix composites exhibiting high strength and toughnessJournal of Materials Science, 1982
- High-strength silicon carbide fibre-reinforced glass-matrix compositesJournal of Materials Science, 1980