Abstract
The frequency dependent complex impedance and dielectric behavior of (100-x) La0.7Ca0.3MnO3 (LCMO)/(x) BaTiO3 (BTO) has been investigated at room temperature (300K). Separate contributions from various factors such as bulk effect, grain boundary and interface effect have been established by fitting the cole-cole function of real and imaginary part of complex impedance. Dielectric data were well fitted in the frequency domain with modified Curie-Von Schweider (CS) functions. Both formalisms support a non-Debye relaxation process in the composites.