Gold extraction from seawater or electronic waste leachate using adsorbents promises sustainable utilization, however the trace amounts of gold in these sources and competitive adsorption from other ions make a significant challenge to achieving both high extraction capacity and precise selectivity. Here, we report a maximum gold extraction capacity of approximately 4.44 g g-1, achieved at gold concentrations as low as 0~10 ppm, using low-oxygen Ti3C2Tx membranes synthesized with a modified method. Remarkably, the Ti3C2Tx membranes efficiently extract gold ions with capacities exceeding 1.44 g g-1, even at ppb levels. These capacities of the Ti3C2Tx at low gold concentrations, are two to three times superior to current state-of-the-art adsorbents, including those of the reported Ti3C2Tx. This efficient extraction yields high-purity and easily peelable gold foil directly from the surface of the Ti3C2Tx membrane. The exceptional extraction performance is attributed to our modified Ti3C2Tx synthesis method, which crucially involves low-temperature and oxygen-deficient conditions to control oxygen content during exfoliation of Ti3C2Tx flakes, enhancing gold adsorption and reduction capabilities. In cross-flow tests with complex multi-ion solutions and real seawater, our Ti3C2Tx membranes demonstrate excellent gold extraction selectivity, showing their practical value for extracting trace amounts of gold from solutions and seawater.