Compositionally uniform (in depth and in lateral position) chemically vapor deposited films were deposited on 200 mm Si wafers in a single‐wafer reactor using chemistry. A process window was found to produce highly uniform compositions in the range of , regardless of the nucleation surface, or poly‐Si. 900°C annealing in of such films deposited on P‐doped poly‐Si resulted in a uniform reduction of to a value of 2.1 to 2.2. In contrast, as deposited films which are Si‐poor at the interface, were found to develop a high concentration of Si in the middle layer of the annealed structure. The as‐deposited resistivity was found to increase linearly with with a value of ∼750 μΩ · cm for . Upon annealing, the resistivities decreased to values in the range of 80 to 110 μΩ · cm. The as‐deposited films were predominantly in the hexagonal structure of , which transformed to the tetragonal structure upon annealing at temperatures higher than 600°C. As‐deposited stresses were in the range of (1.3 to 1.6) · 1010dyne/cm2, and upon annealing reduced to ∼1 · 1010 dyne/cm2. The films had a very good step coverage even at high aspect ratios and did not crack or peel off upon annealing. The films contained relatively low levels of impurities: and . This systematic study reviews the correlations between the structural, compositional, mechanical, and electrical properties of the as‐deposited and the annealed silicide films.