Degradation of Nile blue sulphate dye onto iron oxide nanoparticles: Kinetic study, identification of reaction intermediates, and proposed mechanistic pathways
- 29 May 2018
- journal article
- research article
- Published by Wiley in Asia-Pacific Journal of Chemical Engineering
- Vol. 13 (3) , e2200
Abstract
Iron oxide nanoparticles (Fe3O4 NPs) were synthesized and characterized using Fourier transform infrared spectroscopy, X‐ray diffraction, vibrating sample magnetometer, nitrogen adsorption–desorption, and transmission electron microscopy. Vibrating sample magnetometer analysis confirmed the superparamagnetic behavior of Fe3O4 NPs with a specific saturation magnetization value 43 emu g−1. Synthesized Fe3O4 NPs exhibited surface area 52 m2 g−1 with pore volume 0.0729 cc g−1 and average pore diameter 5.528 nm. The degradation efficiency of Nile blue sulphate (NBS) dye onto Fe3O4 NPs was 86.8% with total organic carbon removal and chemical oxygen demand conversion of 65.6% and 55.9%, respectively, at 5mM H2O2 and 50 mg l−1 of NBS dye concentration for 12 min of reaction time. Rate of degradation of dye onto Fe3O4 NPs followed second‐order kinetic rate equation with high value of regression coefficient (R2 = 0.997) at 303 K. The low activation energy (19.16 kJ mol−1) obtained from Arrhenius plot showed that of Fe3O4 NPs have high catalytic activity towards the degradation of NBS dye during oxidation process. The intermediate products formed during degradation of NBS dye were detected by liquid chromatography–mass spectrometry experiment, and 11 numbers of fragments were detected on the basis of mass to charge ratio (m/z) at 24.186 min. The degradation of NBS dye was attributed to formation of intermediates from destruction of conjugated structure of dye and transformation of these intermediates into small molecules, which were further mineralized to water and carbon dioxide.Keywords
This publication has 43 references indexed in Scilit:
- Synthesis, Surface Modification and Characterisation of Biocompatible Magnetic Iron Oxide Nanoparticles for Biomedical ApplicationsMolecules, 2013
- Photo-catalytic degradation of toxic dye amaranth on TiO2/UV in aqueous suspensionsMaterials Science and Engineering: C, 2012
- Degradation of phenol by heterogeneous Fenton reaction using multi-walled carbon nanotube supported Fe2O3 catalystsColloids and Surfaces A: Physicochemical and Engineering Aspects, 2009
- Highly solar active Fe(III) immobilised alumina for the degradation of Acid Violet 7Solar Energy Materials and Solar Cells, 2008
- Experimental Design to Optimize the Oxidation of Orange II Dye Solution Using a Clay-based Fenton-like CatalystIndustrial & Engineering Chemistry Research, 2007
- Adsorption kinetic, thermodynamic and desorption studies of C.I. Reactive Black 5 on a novel photoassisted Fenton catalystDyes and Pigments, 2007
- Study of kinetic parameters related to the degradation of an industrial effluent using Fenton-like reactionsJournal of Photochemistry and Photobiology A: Chemistry, 2006
- Oxidation of commercial reactive azo dye aqueous solutions by the photo-Fenton and Fenton-like processesJournal of Photochemistry and Photobiology A: Chemistry, 2003
- Equilibrium and kinetic modelling of biosorption of Remazol Black B by Rhizopus arrhizus in a batch system: effect of temperatureProcess Biochemistry, 2000
- China clay as an adsorbent for dye house wastewatersEnvironmental Technology, 1992