Microstructural, mechanical and tribological characterization of Co–20 wt% WC composite elaborated by solid-phase sintering of Co–W–C powders mixture
Authors:
- 25 August 2021
- journal article
- research article
- Published by SAGE Publications in Tribology - Materials, Surfaces & Interfaces
- Vol. 16 (3) , 202-210
Abstract
In this paper, we present the synthesis of a Co–WC compound with 80% of cobalt in a single step by sintering powders compacted and previously milled for 10 h. The purpose of this work is to obtain a fine structure avoiding the formation of mixed carbides and reducing the WC/WC interfaces. The original powder mixture contained 80 wt% Co, 13 wt% W and 7 wt% C. The Co–20% WC metal matrix composite was successfully synthesized with a very fine and homogeneous structure. It presented a good wear resistance and showed that increasing the applied load from 5 to 10 N led to decrease the friction coefficient from 0.52 to 0.35 (sample speed = 10 cm/s) and from 0.90 to 0.61 (sample speed = 20 cm/s). The hardness and Young's modulus of Co phase and WC grains, measured by nanoindentation technique, were 0.78/79.9 and 5.78/164.6 GPa, respectively.Keywords
This publication has 27 references indexed in Scilit:
- Effect of sintering atmosphere on microwave prepared WC–8wt.%Co cemented carbideInternational Journal of Refractory Metals and Hard Materials, 2013
- Interdiffusion and Atomic Mobility for Face-Centered Cubic (FCC) Co-W AlloysMetallurgical and Materials Transactions A, 2013
- Thermal oxidation behavior of WC–Co hard metal machining tool tip scrapsJournal of Materials Processing Technology, 2012
- Comparison of the friction and wear behaviour of WC–Ni–Co–Cr and WC–Co hardmetals in contact with steel at high temperaturesWear, 2012
- Nano crystalline tungsten mono-carbide synthesis from tungstic acid and polyacrylonitrile mixed powderJournal of the Ceramic Society of Japan, 2012
- Comparison of the oxidation behaviour of WC–Co and WC–Ni–Co–Cr cemented carbidesCorrosion Science, 2011
- Evolution of the WC grain shape in WC–Co alloys during sintering: Cumulated effect of the Cr addition and of the C contentInternational Journal of Refractory Metals and Hard Materials, 2009
- Preparation of WC-WB-W2B Composites from B4C-W-WC Powders and their Mechanical PropertiesMATERIALS TRANSACTIONS, 2002
- Oxidation of WC-Co, WC-Ni and WC-Co-Ni hard metals in the temperature range 500–800 °CInternational Journal of Refractory Metals and Hard Materials, 1996
- The oxidation of cobalt in air from room temperature to 467 COxidation of Metals, 1981