Influence of Temperature and Exposure Time Upon Calcareous Deposits
Authors:
- M. M. KunjapurMKM. M. Kunjapur
- W. H. HarttWHW. H. Hartt
- 1 November 1987
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 43 (11) , 674-679
Abstract
Experiments have been performed where cylindrical 1018 steel specimens were polarized to –0.900 V (SCE) in natural seawater at 24 and 3 C with rotation speeds of 0 and 0.83 Hz. The nature of the calcareous deposits that formed was characterized first by monitoring current density (CD) during the experiments and secondly by post-test SEM investigation of deposit morphology and thickness and by EEDS analysis of deposit composition. The dependence of cathodic CD and film composition upon temperature and exposure time has been established, and the observed trends have been interpreted in terms of (1) the temperature dependence of the solubility limit and the relative nucleation and growth rates for calcium- and magnesium-rich phases and (2) possible electrical conductive behavior of magnesium-rich deposits.Keywords
This publication has 6 references indexed in Scilit:
- Calcareous Deposits on Metal Surfaces in Seawater—A Critical ReviewCorrosion, 1984
- An Initial Investigation of Calcareous Deposits Upon Cathodic Steel Surfaces in Sea WaterCorrosion, 1981
- Calcium carbonate retention in supersaturated seawaterAmerican Journal of Science, 1973
- CALCIUM CARBONATE SATURATION IN SEAWATER: EFFECTS OF DISSOLVED ORGANIC MATTER1Limnology and Oceanography, 1970
- Current density required for cathodic protectionJournal of Chemical Technology & Biotechnology, 1965
- Cathodic Protection of Steel in Sea Water With Magnesium AnodesCorrosion, 1948