Evaluating chemical and surface stability of thermoformed and 3D-printed clear aligners after intraoral exposure
Open Access
- 2 April 2026
- journal article
- research article
- Published by Public Library of Science (PLoS) in PLOS ONE
- Vol. 21 (4) , e0345179
Abstract
Introduction: Align Technology, Inc. is a leading manufacturer of orthodontic aligners, using SmartTrack TM (LD30), a multilayer aromatic thermoplastic polyurethane/copolyester, and the vacuum thermoforming process. Recently, direct 3D printing using Tera Harz TC-85 DAC resin has also been explored for the production of aligners. Both aligner materials are exposed to physical and chemical aging in the oral cavity. This study evaluates the chemical aging of these materials after 7 and 14 days of exposure to the oral environment, using Optical Microscopy, Raman spectroscopy, X-ray fluorescence (XRF), and X-ray diffraction (XRD). Materials and methods: Invisalign® aligners (SmartTrack TM LD30) and 3D printed aligners (Tera Harz TC-85 DAC) were worn by 20 patients for 7 ( t 1 ) and 14 days ( t 2 ). The aligners were characterized initially ( t 0 ) using Optical Microscopy, Raman spectroscopy, XRF, and XRD. After t 1 and t 2 , each aligner was reanalyzed at three locations: right and left first molars ( p 1 and p 2 ), and central incisor ( p 3 ). The results were compared with never-worn aligners ( t 0 , n = 3). Results: Both materials showed high homogeneity across all locations ( p 1 , p 2 , p 3 ) and time points, indicating uniform performance after oral exposure. PCA analysis performed on Raman spectra revealed no significant chemical changes in the surface composition after 7–14 days of use. Discussion and conclusions: The results demonstrated that exposure to the oral environment for up to 14 days did not significantly alter the surface chemistry of either aligner material. These findings are consistent with recent literature, suggesting that short-term intra-oral exposure does not affect aligner materials’ chemical stability.Keywords
This publication has 52 references indexed in Scilit:
- Chemical analysis and performance evaluation of ClearCorrect® aligners as received and after intraoral use: Implications for durability, aesthetics, and patient safetyDental Materials, 2024
- Physiochemical and mechanical characterisation of orthodontic 3D printed aligner material made of shape memory polymers (4D aligner material)Journal of the Mechanical Behavior of Biomedical Materials, 2023
- Alterations in the surface roughness and porosity parameters of directly printed and Invisalign aligners after 1 week of intraoral usage: An in vivo prospective investigationAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2023
- Cytotoxicity and estrogenicity of a novel 3-dimensional printed orthodontic alignerAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2022
- Changes in surface morphology, chemical and mechanical properties of clear aligners during intraoral usage: A systematic review and meta-analysisInternational Orthodontics, 2022
- Changes in mechanical properties, surface morphology, structure, and composition of Invisalign material in the oral environmentAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2020
- Mechanical and geometric properties of thermoformed and 3D printed clear dental alignersAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2019
- A new insight into polyurethane foam deterioration – the use of Raman microscopy for the evaluation of long‐term storage conditionsJournal of Raman Spectroscopy, 2016
- Investigation of Ageing Mechanisms in Thermoplastic Polyurethanes by Means of IR and Raman SpectroscopyMacromolecular Symposia, 2014
- Structural conformation and leaching from in vitro aged and retrieved Invisalign appliancesAmerican Journal of Orthodontics and Dentofacial Orthopedics, 2004