Abstract
Aims: This in vitro study aimed to compare the fracture resistance of teeth restored with different provisional materials. Materials and methods: Twenty single-rooted human incisors were prepared and randomly divided into four groups (n = 5), according to the provisional restorative material used: Coltosol, IRM, Vidrion R Plus, and J-Temp. A standardized 4 mm thickness of provisional material was placed in each cavity, and specimens were embedded in acrylic resin cylinders, maintaining 3 mm of the coronal root exposed to simulate biological conditions. Fracture resistance was evaluated using a universal testing machine with a 135° load angle, simulating occlusal contact. Load at fracture (N), load application time (s), and displacement (mm) were recorded. Data were analyzed using one-way ANOVA and Tukey’s post hoc test (sig 5%). Results: No statistically significant differences were found among the groups for load application time and displacement (p > 0.05). However, J-Temp exhibited significantly higher fracture resistance than all other materials (p < 0.05). Conclusion: These findings suggest that J-Temp not only ensures adequate provisional sealing but also reinforces coronal structure, making it a promising alternative in cases requiring higher mechanical performance. Further long-term clinical studies are warranted to confirm its effectiveness under oral conditions.

This publication has 19 references indexed in Scilit: