Difference of near-interface strain in SiO2 between thermal oxides grown on 4H-SiC by dry-O2 oxidation and H2O oxidation characterized by infrared spectroscopy
- 10 April 2017
- journal article
- research article
- Published by AIP Publishing in Applied Physics Letters
- Vol. 110 (15)
Abstract
Structural difference of near-interface oxides at thermally grown SiO2/4H-SiC interfaces between dry-O2 oxidation and H2O oxidation was investigated using infrared spectroscopy for both on Si- and C-faces. We found that H2O oxidation results in a significant reduction of the intrinsic strain of SiO2 in the near-interface region compared to dry-O2 oxidation, while such strain was not affected by the change of oxidation temperature and O2 partial pressure in the case of dry-O2 oxidation. The peak broadness observed in the near-interface region was also smaller for H2O oxidation than for dry-O2 oxidation, which indicated a formation of an oxide with more uniformity in microscopic structures. A strong correlation between the strain of near-interface oxides and the formation of near-interface oxide traps was suggested from the clear difference of the characteristics of metal-oxide-semiconductor capacitors fabricated with different oxidants.Keywords
Funding Information
- New Energy and Industrial Technology Development Organization (14101705)
- Japan Society for the Promotion of Science (15J10704, 26630291)
This publication has 30 references indexed in Scilit:
- First-Principles Study on Interlayer States at the 4H-SiC/SiO2Interface and the Effect of Oxygen-Related DefectsJournal of the Physical Society of Japan, 2016
- First principles study of SiC/SiO2 interfaces towards future power devices2014
- A New-Type of Defect Generation at a 4H-SiC/SiO2 Interface by Oxidation Induced Compressive StrainMaterials Science Forum, 2013
- Limiting mechanism of inversion channel mobility in Al-implanted lateral 4H-SiC metal-oxide semiconductor field-effect transistorsApplied Physics Letters, 2011
- Inversion layer carrier concentration and mobility in 4H–SiC metal-oxide-semiconductor field-effect transistorsJournal of Applied Physics, 2010
- The mechanism of defect creation and passivation at the SiC/SiO2interfaceJournal of Physics D: Applied Physics, 2007
- Graphitic features on SiC surface following oxidation and etching using surface enhanced Raman spectroscopyApplied Physics Letters, 2004
- SiC power-switching devices-the second electronics revolution?Proceedings of the IEEE, 2002
- Intrinsic SiC/SiO2 Interface StatesPhysica Status Solidi (a), 1997
- Status of silicon carbide (SiC) as a wide-bandgap semiconductor for high-temperature applications: A reviewSolid-State Electronics, 1996