Protective and Nonprotective Behavior of 11% Cr Steel in O[sub 2]+H[sub 2]O Environment at 450-700°C
Authors:
- 1 January 2004
- journal article
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 151 (7) , B394-B398
Abstract
The oxidation of X20 steel (CrMoV 11 1) in dry O2O2 and O2+10O2+10 or 40%H2O40%H2O was investigated at 450-700°C. The flow rate was 2.5 cm/s and the exposure time was 168 h. The oxidized samples were investigated gravimetrically and by a number of surface analytical techniques including environmental scanning electron microscopy/energy-dispersive X-ray, grazing incidence X-ray diffraction, and glow discharge optical emission spectroscopy. The oxidation behavior was strongly influenced by temperature and pH2O.pH2O. In dry O2O2 the scale was protective up to 700°C, the chromium concentration in the scale increasing with temperature. In O2+H2OO2+H2O environment chromium was lost by vaporization of CrO2(OH)2,CrO2(OH)2, resulting in a deterioration of the ability of the oxide to protect the metal. This resulted in rapid oxidation in O2+40%H2OO2+40%H2O at high temperature (650 and 700°C) and at low temperature (500°C), forming a thick duplex (Fe2O3/Fe2CrO4)(Fe2O3/Fe2CrO4) scale. In the intermediate temperature range (550-600°C) the rate of oxidation was not increased. The results are interpreted in terms of the ability of the material to compensate for chromium vaporization by supplying chromium to the protective oxide by diffusion. © 2004 The Electrochemical Society. All rights reserved.Keywords
This publication has 8 references indexed in Scilit:
- The high temperature oxidation of 11% chromium steel: Part II - Influence of flow rateMaterials and Corrosion, 2002
- The high temperature oxidation of 11% chromium steel: Part I - Influence of pH2OMaterials and Corrosion, 2002
- Field test corrosion experiments in Denmark with biomass fuels. Part 2: Co-firing of straw and coalMaterials and Corrosion, 2002
- Corrosion of TP347H FG stainless steel in a biomass fired PF utility boilerJournal of Materials Science, 2001
- Corrosion of HR3C heat exchanger alloy in a biomass fired PF utility boilerMaterials and Corrosion, 2000
- Influence of chromium diffusion and different surface finishes on the oxidation behaviour of chromium steelsMaterials at High Temperatures, 2000
- In-situ corrosion investigation at Masnedø CHP plant - a straw-fired power plantMaterials and Corrosion, 1999
- Indication of Chromium Oxide Hydroxide Evaporation During Oxidation of 304L at 873 K in the Presence of 10% Water VaporOxidation of Metals, 1999