Interdiffusion coefficients (D) were measured from 300 to 600 °C using an angle lapping technique and electron microprobe analysis. The influence of the binary composition, temperature, and Hg overpressure was studied. There is a significant difference in the behavior of D in the higher and lower temperature regions. At higher temperatures (T≥450 °C), D is a strong function of composition and temperature and is insensitive to the Hg overpressure. At lower temperatures (T<450 °C), we observe the following trends with decreasing temperature: (i) the activation energy decreases, (ii) D is less dependent on X (X is the CdTe mole fraction), and (iii) D depends on Hg overpressure. Based on an analysis of our interdiffusion data, we propose a dual mechanism for higher temperatures with a vacancy and an interstitial mechanism dominating at low and high X values, respectively, and an interstitial mechanism at lower temperatures.