Abstract
Measurements of S′ precipitate dimensions in Al-4·1 Cu-1·6 Mg-0·1 Mn (wt%) alloy for times up to 10 000 h at 200°C are shown to give coarsening rates in good accord with previous results in the range 260 to 300°C and at 190°C. The three sets of results are represented well by KT = K 0 exp (-Q/RT) with Q = 175 kJ mol-1 and K 0 = 3·2 10-9 m3 Ks-1 where K = (2dV/dA)3 in which V and A are the mean volume and surface area of the S′ lath precipitates respectively.