Tensile properties of partially austenitised and austempered ductile irons with dual matrix structures
Authors:
- V. KilicliV. Kilicli
- M. ErdoganMEM. Erdogan
- 1 August 2006
- journal article
- Published by SAGE Publications in Materials Science and Technology
- Vol. 22 (8) , 919-928
Abstract
In the present study, an unalloyed ductile iron containing Fe–3·50C–2·63Si–0·318Mn–0.047Mg (wt-%) were intercritically austenitised (partially austenitised) in two phase region α+ γ at various temperatures of 795, 805, 815 and 830°C for 20 min and then quenched into salt bath held at austempering temperature of 365°C for various times to obtain different ausferrite volume fractions (AFVFs). Results showed that dual matrix structure containing proeutectoid ferrite, new ferrite (also called epitaxial ferrite) and ausferrite (bainitic ferrite+high carbon austenite, which is retained or stabilised austenite) has been developed. Within each of the austempered series in α+ γ temperature range, new ferrite volume fraction increased with increasing intercritical austenitising temperature (ICAT). Although, transforming percentage of new ferrite from parent austenite present at ICAT increased with decreasing ICAT. Some specimens were also conventionally austempered from 900°C for comparison. The new ferrite was absent in these samples. The volume fraction of proeutectoid ferrite, new ferrite and ausferrite can be controlled to determine the strength and ductility. Austempered specimens in α+ γ temperature range exhibited much greater ductility than conventionally austempered ones. The tensile strength increased while ductility decreased with increasing AFVF. On the other hand, the ductility increased with increasing proeutectoid ferrite and new ferrite volume fractions at the expense of strength. The specimen with ∼47·2%AFVF exhibited the best combination of high strength and ductility. The strength and ductility of this material is much higher than that of ferritic grades. Its strength is at the same level as while ductility almost more than four times higher than that of pearlitic grades. Meanwhile, the specimen with ∼ 75%AFVF exhibited the best combination of high strength and ductility compared with those of pearlitic grades. The strength of this material is much higher and its ductility is almost more than two times higher than that of pearlitic grades yet slightly lower than that of ferritic grades. This material also meets the requirements for the strength of quenched and tempered grades and its ductility is higher than that of this grade.Keywords
This publication has 25 references indexed in Scilit:
- The effect of austempering time on mechanical properties of a ductile ironScandinavian Journal of Metallurgy, 2001
- INFLUENCE OF AUSTEMPERING TEMPERATURE ON FRACTURE TOUGHNESS OF A LOW MANGANESE AUSTEMPERED DUCTILE IRON (ADI)Materials and Manufacturing Processes, 2001
- The control of the chemical composition, microstructure and mechanical properties of beinite ductile iron for liner platesJournal of Materials Processing Technology, 1999
- Influence of molybdenum on austempering behaviour of ductile iron Part 1 – Austempering kinetics and mechanical properties of ductile iron containing 0·13%MoMaterials Science and Technology, 1999
- Effect of silicon content on transformation kinetics of austempered ductile ironMaterials Science and Technology, 1998
- Effect of Composition and Heat Treatment Parameters on the Characteristics of Austempered Ductile IronsCanadian Metallurgical Quarterly, 1997
- The austempering kinetics and mechanical properties of an austempered Cu–Ni–Mo–Mn alloyed ductile ironJournal of Materials Science, 1997
- Influence of austenitising temperature on austempering kinetics of high manganese alloyed ductile cast ironMaterials Science and Technology, 1995
- Influence of heat treatments on microstructure of austempered ductile ironMaterials Science and Technology, 1994
- Austempering of low manganese ductile ironsMaterials Science and Technology, 1993