Chemical-mechanical photoresist drying in supercritical carbon dioxide with hydrocarbon surfactants
- 1 March 2004
- journal article
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 22 (2) , 818-825
Abstract
No abstract availableKeywords
This publication has 38 references indexed in Scilit:
- Deposition of Conformal Copper and Nickel Films from Supercritical Carbon DioxideScience, 2001
- Effect of Pressure on the Static Forces of Micron-Scale Particle AdhesionIndustrial & Engineering Chemistry Research, 2000
- Nanoscale Casting Using Supercritical FluidThe Journal of Physical Chemistry B, 1999
- High-Aspect-Ratio Nanometer-Pattern Fabrication Using Fullerene-Incorporated Nanocomposite Resists for Dry-Etching ApplicationJapanese Journal of Applied Physics, 1997
- Sub-0.1 µm Patterning with High Aspect Ratio of 5 Achieved by Preventing Pattern CollapseJapanese Journal of Applied Physics, 1996
- Structural analysis of silica aerogelsJournal of Non-Crystalline Solids, 1995
- Prevention of Resist Pattern Collapse by Flood Exposure during Rinse ProcessJapanese Journal of Applied Physics, 1994
- Prevention of Resist Pattern Collapse by Resist Heating during RinsingJournal of the Electrochemical Society, 1994
- Freeze-Drying Process to Avoid Resist Pattern CollapseJapanese Journal of Applied Physics, 1993
- Mechanism of Resist Pattern Collapse during Development ProcessJapanese Journal of Applied Physics, 1993