Abstract
Incorporation of saccharin molecules has been studied during the galvanostatic deposition of 2.45 CoFe alloys. The results indicate that the incorporation rate is strongly dependent on the concentration of saccharin in the plating solution. This dependence showed a pronounced maximum at , which is a result with significant practical implications. A simple physical model was developed to describe this dependence, having an excellent qualitative agreement with experimental data. The corrosion properties and surface roughness of CoFe deposits were found to be a strong function of saccharin concentration in the plating solution, i.e., the incorporation rate of saccharin molecules.

This publication has 24 references indexed in Scilit: