Steam Degradation of Ytterbium Disilicate Environmental Barrier Coatings: Effect of Composition, Microstructure and Temperature
Open Access
- 20 October 2022
- journal article
- research article
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 32 (1) , 29-45
Abstract
Recession of environmental barrier coatings (EBC) in environments containing steam is a pressing concern that requires further research before their implementation in gas turbine engines can be realized. In this work, free-standing plasma-sprayed Yb2Si2O7 coatings were exposed to flowing steam at 1350 and 1400 °C for 96 h. Three samples were investigated, one coating with a low porosity level ( < 3%) and 1 wt.% Al2O3 representing traditional EBCs porosity levels; and two coatings with higher porosity levels (~ 20%) representing abradable EBCs. Phase composition and microstructural evolution were studied in order to reveal the underlying mechanism for the interaction between high temperature steam and ytterbium disilicate. The results show depletion of Yb2SiO5 near the surface and formation of ytterbium garnet (Yb3Al5O12) on top of all three coatings due to the reaction with gaseous Al-containing impurities coming from the alumina furnace tubes. The 1 wt.% Al2O3 added to the EBC sample exacerbated the formation of garnet at 1400 °C compared to the abradable samples, which presented lower quantities of garnet. Additionally, inter-splat boundaries were visible after exposure, indicating preferential ingress of gaseous Al-containing impurities through the splat boundaries.Keywords
This publication has 52 references indexed in Scilit:
- Fiji: an open-source platform for biological-image analysisNature Methods, 2012
- A Method for Assessing Reactions of Water Vapor with Materials in High‐Speed, High‐Temperature FlowJournal of the American Ceramic Society, 2011
- Calcium–Magnesium Alumino‐Silicate Interaction with Yttrium Monosilicate Environmental Barrier CoatingsJournal of the American Ceramic Society, 2010
- Ceramic Gas Turbine Development: Need for a 10Year PlanJournal of Engineering for Gas Turbines and Power, 2009
- Comparison of Water Vapor Corrosion Behaviors of Ln2Si2O7 (Ln=Yb and Lu) and ASiO4 (A=Ti, Zr and Hf) EBC'sKey Engineering Materials, 2006
- Development of Oxide‐Based EBC for Silicon NitrideInternational Journal of Applied Ceramic Technology, 2004
- SiC Recession Caused by SiO 2 Scale Volatility under Combustion Conditions: II, Thermodynamics and Gaseous‐Diffusion ModelJournal of the American Ceramic Society, 1999
- Mass Spectrometric Identification of Si–O–H( g ) Species from the Reaction of Silica with Water Vapor at Atmospheric PressureJournal of the American Ceramic Society, 1997
- Oxidation Kinetics of Chemically Vapor‐Deposited Silicon Carbide in Wet OxygenJournal of the American Ceramic Society, 1994
- Phase Equilibria and Properties of Glasses in the Al2O3-Yb2O3-SiO2 SystemJournal of the Ceramic Society of Japan, 1993