Atomic Layer Deposition of Alumina onto Carbon Fibers
- 18 February 2011
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 94 (7) , 2014-2022
Abstract
Bundles of carbon fibers were successfully coated with alumina by atomic layer deposition via sequential exposures to trimethylaluminum and water at 77°C. Fibers were not damaged by this procedure. Scanning electron microscopy (SEM) images revealed that individual filaments were coated separately with a smooth layer; no bridging of fibers was observed. Transmission electron microscopy (TEM) and SEM images indicate that the coating was conformal and adhered well to the fiber surface. The average deposition rate was 0.25±0.02 nm/cycle, calculated from SEM images obtained at various positions of the fibers and of fibers coated with various numbers of cycles. In addition to image analysis, the coating thickness was as well estimated from the elemental composition of selected parts of a fiber bundle that was coated by 450 cycles. Along the fiber axis, the weight fraction of aluminum of the coated fibers varied from 5.3 to 6.5 wt% and perpendicular to the bundle axis it varied from 4.8 to 7.4 wt%. This translates into a variation of the estimated coating thickness along the fiber from 166 to 126 nm and perpendicular to it from 114 to 183 nm. One can estimate independently an average coating thickness from the analysis of SEM images of this specific bundle of 126 nm. The alumina coating improved oxidation resistance of the carbon fiber significantly. The oxidation onset temperature was 600°C for fibers coated with a 30‐nm‐thick layer of alumina and increased gradually with increasing coating thickness up to 660°C at a thickness of 120 nm. On the other hand, uncoated fibers started to oxidize already at 300°C.Keywords
This publication has 50 references indexed in Scilit:
- Carbon fibre-reinforced magnesium: Improvement of bending strength by nanodesign of boron nitride interlayersMaterials Chemistry and Physics, 2007
- Interface Design for Oxidation‐Resistant Ceramic CompositesJournal of the American Ceramic Society, 2002
- Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVISolid State Ionics, 2001
- Interface Engineering of Carbon-Fiber Reinforced Mg-Al AlloysAdvanced Engineering Materials, 2000
- The CVD of pyrolytic carbon and titanium diboride coatings on carbon fibre yarns for use in aluminium-based compositesSurface and Coatings Technology, 1997
- Oxidation protection for carbon fibre compositesJournal of Materials Science, 1996
- Oxidation protection of carbon fibers by coatingsCarbon, 1995
- Property-structure characterisation of a continuous fine alumina-silica fibreComposites Science and Technology, 1990
- The oxidative stability of carbon fibre reinforced glass-matrix compositesJournal of Materials Science, 1988
- Creep behaviour and structural characterization at high temperatures of Nicalon SiC fibresJournal of Materials Science, 1984