High Temperature Oxidation and Corrosion of Silicon-Based Non-Oxide Ceramics
Authors:
- 20 October 1999
- journal article
- Published by ASME International in Journal of Engineering for Gas Turbines and Power
- Vol. 122 (1) , 13-18
Abstract
The present study is focussed on the oxidation behavior of nonoxide silicon-based ceramics. Various Si3N4 and SiC ceramics were examined after long term oxidation tests (up to 5000 h) at 1500°C in ambient air. The damage mechanisms were discussed on the basis of a comprehensive chemical and microstructural analysis of the materials after the oxidation tests. The diffusion of oxygen into the material and its further reaction in the bulk of the material were found to be the most critical factors during long term oxidation treatment at elevated temperatures. However, the resulting damage in the microstructure of the materials can be significantly reduced by purposeful microstructural engineering. Using Si3N4/SiC and Si3N4/MoSi2 composite materials provides the possibility to improve the high temperature stability. [S0742-4795(00)00301-X]Keywords
This publication has 21 references indexed in Scilit:
- Long-Term Behaviour of SiC/Si3N4-Nanocomposites at 1400-1500° CKey Engineering Materials, 1997
- Silicon Nitride Composites Materials with an Improved High Temperature Oxidation Resistance1997
- Influence of Molybdenum Silicide Additions on High‐Temperature Oxidation Resistance of Silicon Nitride MaterialsJournal of the American Ceramic Society, 1996
- Differences in Creep Performance of a HIPed Silicon Nitride in Ambient air and Inert Environments1995
- Problems and prospects of silicon nitride materials for applications at temperatures above 1400 °CHigh Temperatures-High Pressures, 1995
- Creep and Stress Rupture Behavior of an Advanced Silicon Nitride: Part III, Stress Rupture and the Monkman–Grant RelationshipJournal of the American Ceramic Society, 1994
- Creep and Stress Rupture Behavior of an Advanced Silicon Nitride: Part I, Experimental ObservationsJournal of the American Ceramic Society, 1994
- Role of Oxidation in the Time‐Dependent Failure Behavior of Hot Isostatically Pressed Silicon Nitride at 1370°CJournal of the American Ceramic Society, 1993
- Compressive Creep and Oxidation Resistance of an Si 3 N 4 Material Fabricated in the System Si 3 N 4 ‐Si 2 N 2 O‐Y 2 Si 2 O 7Journal of the American Ceramic Society, 1983
- Strengthening of a Sintered Silicon Nitride by a Post‐Fabrication Heat TreatmentJournal of the American Ceramic Society, 1982