Abstract
The synergistic roles of boron carbide and carbon additions in the enhanced densification of zirconium diboride (ZrB 2 ) by pressureless sintering have been studied. ZrB 2 was sintered to >99% relative density at 1900°C. The combination of 2 wt% boron carbide and 1 wt% carbon promoted densification by removing surface oxide impurities (ZrO 2 and B 2 O 3 ) and inhibiting grain growth. Four‐point bending strength (473±43 MPa), Vickers' microhardness (19.6±0.4 GPa), fracture toughness (3.5±0.6 MPa·m 1/2 ), and Young's modulus (507 GPa) were measured. Thermal gravimetry showed that the combination of additives did not have an adverse effect on the oxidation behavior.