Accumulation of Creep Damage in a Siliconized Silicon Carbide
Authors:
- 1 June 1988
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 71 (6) , 472-477
Abstract
The accumulation of creep damage in a siliconized silicon carbide was investigated as a function of applied stress, creep strain, and microstructure. At 1100°C, creep damage was observed to accompany deformation in specimens tested to creep strains greater than 0.10%, under applied stresses greater than 137 MPa. At low creep strains, creep damage occurred in regions of the microstructure of high silicon carbide content. As deformation progressed, creep damage extended into regions of the microstructure of lower silicon carbide content. The area density and area fraction of cavities were found to increase linearly with creep strain. From these results, a threshold stress for the formation of creep damage was determined to be 132 MPa at 1100°C. It was suggested that the formation of creep damage was controlled by the heterogeneous nucleation of cavities at the silicon‐silicon carbide interface, with the aid of high localized stresses and iron impurities in the silicon phase.Keywords
This publication has 6 references indexed in Scilit:
- Microstructural evolution in reaction-bonded silicon carbideJournal of Materials Science, 1986
- Creep Rupture of Siliconized Silicon Carbide1986
- Estimation of power-law creep parameters from bend test dataJournal of Materials Science, 1986
- Time‐Dependent Strength of Siliconized Silicon Carbide under Stress at 1000° and 1100°CJournal of the American Ceramic Society, 1985
- High‐Temperature Failure of Polycrystalline Alumina: I, Crack NucleationJournal of the American Ceramic Society, 1984
- The Fracture of LiquidsJournal of Applied Physics, 1948